7 Ways to Eliminate Porosity in Your Welds

Porosity is a weld discontinuity that is not as detrimental to structural integrity as cracks, undercut, overlap and lack of fusion. However, it is unsightly and when painted it looks absolutely horrible. Because it does not have sharp ends, porosity does not propagate like a crack. The reason why there are limits to the amount […]