Types of Weld Joints

Welding joints vary widely but can be traced back to a few basic joint types.  Typically we hear terms like fillet weld, butt weld, lap weld or corner weld.  These are all all joints but within these there are variations.  Below we outline the joints and provide a graphical representation.  These joint types are categorized by how the plates come together, and further subcategorized by joint preparation.

BUTT JOINTS

Butt joints consist of placing two plates side by side and joining to create a single piece.  When plate thickness increases, or full penetration is desired, the plates are beveled. These are referred to as groove welds.  Beveling increases the amount of filler metal needed but insures higher strength and proper penetration.

 

Butt Joints

Butt Joints

TEE JOINTS (FILLET WELDS)

The tee joint has variations when a one of the pieces is beveled. As with butt welds, the bevel is used to achieved deeper or full penetration.  It also requires less weld for equal strength on heavier sections.

Tee Weld Joints

 

CORNER WELDS

Corner welds are used to joint plates at 90 degree angles.  Depending on material thickness it can be a straight butt weld, a lap weld, a fillet weld, or a groove weld.

Corner Weld Joints

Corner Joints

 

LAP WELDS

Lap welds are  similar to fillet welds but the the size of the fillet typically reaches the top of one of the pieces.

Lap Joint

Lap Joint

 

EDGE WELDS

Edge Joint

Edge Joint

Please note: I reserve the right to delete comments that are offensive or off-topic.

Leave a Reply to The Welding Guys Cancel reply

Your email address will not be published. Required fields are marked *

5 thoughts on “Types of Weld Joints

  1. Hello
    Why outside-corner fillet weld isn’t proper for box column in steel structure?
    Ì need your technical reasons for that question.
    Thanks.

    • Hello Hanif, can you provide more detail on this question? Is this statically or cyclically loaded? If cyclically loaded, corner joints parallel to the direction of calculated stress between components of built-up members is prohibited by AWS D1.1 This could be due to the susceptibility of crack initiation due to surface or internal discontinuities. If you have access to a weld design engineer this should be brought to him or her and provide a lot more detail.

    • It depends on how the part is loaded and also on the size of theweld. In design, we want joints that are accessible, that minimize the amount of weld metal, and that allow for a strong enough weld to carry the loaded. You don’t always have a choice of joint but rather use whatever is allowed by the geometry of the structure. But, an example of when you would have a choices is joining two plates either on a butt joint or a lap joint. A complete joint penetration (CJP) weld will more than likely provide higher load carrying capacity that two lap joints which would be loaded in shear rather than pure tension. A bit hard to explain with words, but hopefully you get the picture.