Hot Cracking vs Cold Cracking
We recently helped out a customer in troubleshooting weld cracking which they were experiencing frequently. It was determined that cracking on their parts was due to rapid cooling and improperly sized welds. The discussions we had before and after determining the cause were quite interesting. We went over the typical causes for cracking with our […]