Proper Storage of Welding Consumables
Proper storage of both opened and unopened packages of welding consumables is crucial. It should avoid quality issues such as porosity, excessive slag fluidity, rough weld surface, difficult slag removal and more importantly, elevated levels of diffusible hydrogen which can lead to cracking. Adequate storage, handling and re-conditioning of electrodes vary according to type. The […]