Should Heat Input Always Be Kept As Low As Possible?

Many ‘experts’ in the welding industry talk about high heat input as something that should always be avoided.  Unfortunately, this is not good advice.  High heat input can be detrimental in many cases, but other times we want to have higher heat input. Heat input is directly related to amperage and voltage and inversely related […]