Troubleshooting Weld Cracking – The importance of crack location

One of the first steps in analyzing cracks to find their root cause and take corrective action is to categorize the cracks. We categorize cracks based on three elements. Location Direction Timing In today’s article we discuss the importance of crack location when trying to troubleshoot weld cracking. What follows is an excerpt from Weld […]