Despite decades of standards, many shops still weld without a written welding procedure specification (WPS). A common misconception is that if the parameters used meet the conditions for prequalified status, no written procedure is needed. This is not true. The AWS D1.1 Structural Welding Code – Steel explicitly requires written WPSs for all fabrication—whether prequalified […]