Undercut is a welding discontinuity that can be lead to failures. Welding codes govern how much undercut you can have based on whether the application is cyclic or static. Regardless, the aim should be to have no undercut. This guide will walk you through how to identify the causes of undercut, how to to fix it and how to prevent it from happening again.