5 Factors that Contribute to Silica Island Formation in Welds

The formation of silica islands on welds made with the GMAW (mig) and MCAW (metalcore) processes is very common.  For the most part, these silica islands are not a problem.  However, if the weld is to be painted, you better remove these islands. Otherwise, they will eventually pop off and leave an unpainted spot in […]