Hot Cracking of 304 and 304L Stainless Welds
If you’ve ever welded 304 stainless and suddenly found cracks running through your weld, you’re not alone. Many fabricators are shocked when this happens — especially after years of successful welding with 304. In many of the cases we’ve seen, the cause wasn’t the welder, the process, or the settings. The real reason was that […]