Tag Archives: Dissimilar metals
What Filler Metal Should be Used to Weld Carbon Steel to Stainless Steel
And can you use stainless wire to weld carbon steel to carbon steel
It is not uncommon to find fabricating shops that are welding a variety of metals including carbon steel, stainless steel, aluminum and nickel alloys. In many cases some of these materials need to be welded to other types. Once very common situation, especially in automotive applications is welding carbon steel to stainless. One of the […]