7 Variables That Affect Weld Penetration

Getting deeper penetration, or at least adequate penetration is very important in welding. There are a few applications in which we wish to minimize penetration, but in general we always want good penetration. There are many variables that affect penetration, some more than others. It is important to know how each individual variable affects the […]
Dangers of not Maintaining Proper Interpass Temperature

Interpass temperature is the temperature of the base metal in and adjacent to the weld joint prior to depositing and additional pass (weld). Maintaining and measuring interpass temperature should be done carefully. Different materials require different levels of preheat and interpass temperature. For this reason it is extremely important that both prehat and interpass temperature be specified […]
5 Factors that Contribute to Silica Island Formation in Welds
The formation of silica islands on welds made with the GMAW (mig) and MCAW (metalcore) processes is very common. For the most part, these silica islands are not a problem. However, if the weld is to be painted, you better remove these islands. Otherwise, they will eventually pop off and leave an unpainted spot in […]
How to Weld Weathering (CORTEN) Steel

Corten, or COR-TEN, is the trademark name for weathering steels manufactured by U.S. Steel Corporation. Weathering steels are a family of low carbon steel alloys that were specifically developed to provide higher strength and more importantly eliminate the need to paint to protect against the elements (rain, snow, humidity, sun, salt, etc.). A242 and A588 […]
10 Types of Welding Discontinuities Explained

Not all weld discontinuities are weld defects, but all weld defects are discontinuities. Understanding the difference will let you know if you need to scrap a part, repair it or simply add more weld. There are many codes depending on what type of product you are welding on. The codes are used as guidelines by […]
What is Waveform Control and How It Improves Welding

Waveform control is the ability of a welding power source to affect heat input, droplet shape and size, penetration, bead shape and toe wetting by the use of microprocessor controls which manage the welding output. Advances in waveform control technology over the past two decades have provided the ability to weld tough materials successfully. One […]
9 Changes for the New AWS D1.1 Structural Welding Code (Steel) 2020 Edition

The new edition of AWS D1.1 Structural Welding Code (Steel) has been released. If you are looking to get the hard copy you may need to wait a few weeks, but the electronic version is ready for purchase from the American Welding Society (AWS) through their website. There is a significant cost to obtain the […]
How to Qualify a WPS for Welding Stainless to Mild Steel using AWS D1.6

It is very common to weld stainless steel to mild steel. But, when it comes to qualifying a welding procedure it can be somewhat confusing. Do you follow AWS D1.1 (Steel) or do you following AWS D1.6 (Stainless Steel)? Or is there another code or standard you should use? The answer to this question is […]
5 Common Mistakes Made When Estimating the Costs of a Welding Job
When bidding jobs several fabricators end up calculating their costs associated with welding and then double that number to be safe. In some cases, that isn’t even enough. It is important to have a clear understating of how to translate the amount of welding to be done to actual manufacturing costs. One of the biggest […]
Is Weld Strength Affected by Shielding Gas Mix?
Can our selection of shielding gas affect the strength of a weld and other important mechanical properties? Absolutely! The difference is more pronounced when using flux-cored (FCAW) wires than when using mig (GMAW) wires, especially as the wire’s tensile strength goes up. Although we can affect strength by using different gases, what we should be […]