6 Factors That Lead to Cracks in Aluminum Welds
![](https://weldinganswers.com/wp-content/uploads/2023/05/Aluminum-Cracking-760x308.png)
Welding aluminum should not be complicated. That is, if you are welding 6061-T6 (very common) with ER5356 or ER4043 filler metal. Although this alloy is still susceptible to cracking, other aluminum alloys are much more prone to cracking. Below are 6 factors that affect cracking susceptibility when welding aluminum alloys. Thermal stresses: Aluminum has […]