The Outrageous Cost of Poor Fit Up

You will cringe when you read this

In a perfect world we would have perfect fit up every time.  However, as well all know, this isn’t the case.  We mostly think of poor fit up as annoying and the cause of some delays.  But the reality is it can have tremendous impact on our bottom line.  Or, in many cases, compromises the […]

How To Calculate Heat Input From Welding

The vast majority of fabricators are not typically concerned with heat input. For the most part this is OK. But when you are welding on materials whose microstructure can be significantly affected by welding procedures it is important to know about heat input. The reason why heat input is critical in certain applications is because […]