7 Ways To Control Distortion in Welding

Distortion is a nasty problem we experience in welding.  Understanding what causes distortion is important in order to be able to minimize or eliminate it completely.  There are physical and mechanical properties that affect distortion susceptibility of materials.  To learn more about this you can read 4 Material Properties That Affect Distortion.

Larger weld nuggets in butt joints can help in minimizing distortion

Larger weld nuggets in butt joints can help in minimizing distortion

As fabricators we hardly ever get to pick the base material of the welded structure.  However, regardless of a material’s mechanical and physical properties, we can follow a set of rules to minimize or eliminate distortion altogether.  Follow these steps and you’ll be on your way to controlling weldment distortion.

    1. Don’t overweld – the more weld metal we put in the joint the higher the forces causing shrinkage. Don’t lay a 5/16” fillet when a ¼” fillet will do.  If there is a drawing calling out welds stick to the sized called for.  If necessary, invest in weld gages. You can learn how to use them in Proper Use of Weld Gages.
    2. Use intermittent welding – using intermittent welds rather than continuous welds, where design allows it, can save as much as 75% weld metal and significantly reduce shrinkage and distortion. Welding stiffeners to plate is a great place to do this.
    3. Minimize the number of weld passes – the shrinkage caused by each pass is cumulative, thus making it better to fill the same volume in fewer passes, especially when we are welding in the  transverse distortion.

4. Weld near the neutral axis – as you can see in the image below the location of the weld relative to the neutral axis will determine which way the structure will distort. If we can place the weld right at the neutral axis we can effectively control distortion.

Source: Haynes International - Welding and Joining

Source: Haynes International – Welding and Joining

5. Balance welds around the neutral axis – we can’t always change the material thickness to affect where the neutral axis is. In this case, whenever possible, balance the welds around the neutral axis.  This means trying to achieve symmetry.

When designing consider the location of the welds based on the neutral axis

When designing consider the location of the welds based on the neutral axis6.

6. Use backstep technique – this is helpful since the previous weld create a restraint minimizing distortion. This technique may not be feasible in all situations.

7. Preset parts to offset distortion – if we anticipate distortion and can predict which way the welded structure will bend, we can pre-bend the part so that after welding the part is straight.

There are other methods for reducing distortion such as planning the welding sequence accordingly to counteract shrinkage forces.  Peening can also reduce some of the residual stresses.   Preheating and other thermal methods can help as well.

Sources: The Procedure Handbook of Arc Welding, 14th Edition

Haynes International – Welding and Joining (Weld Defects)

Please note: I reserve the right to delete comments that are offensive or off-topic.

Leave a Reply to Gerald Austin Cancel reply

Your email address will not be published. Required fields are marked *

5 thoughts on “7 Ways To Control Distortion in Welding