Proper Storage of Welding Consumables

How to store stick electrodes, and mig, flux-cored and metal-cored wires

Proper storage of both opened and unopened packages of welding consumables is crucial. It should avoid quality issues such as porosity, excessive slag fluidity, rough weld surface, difficult slag removal and more importantly, elevated levels of diffusible hydrogen which can lead to cracking.

Welding consumables should be stored in their original unopened packaging in an area shielded from the elements.

Adequate storage, handling and re-conditioning of electrodes vary according to type.  The summary below provides guidelines as to the proper storage of stick electrodes, flux-cored wires, metal-cored wires, and solid wires (mig wire and tig cut length).

 

STICK ELECTRODES

Low Hydrogen Electrodes – classified per AWS as EXX15-X, EXX16-X, and EXX18-X

 

These electrodes must be dry to perform adequately. Manufacturers typically supply these electrodes in hermetically sealed containers which provide proper protection under good storage conditions.  Open containers of low hydrogen electrodes must be stored in a cabinet at 250F – 300F.

Moisture resistant coatings (“R” designation) have higher resistance to moisture pick up, but should still be stored in the same manner.  The “R” designation allows for more exposure time before the electrode needs to be re-dried.  It is recommended that low hydrogen electrodes without the “R” designation be supplied twice per shift to stay below the permissible 4 hours of exposure.  AWS D1.1 Structural Welding Code specifies allowable atmospheric exposure in Table 5.1 which can be seen below.

Low hydrogen electrodes may be re-dried if they exceed exposure limits following the manufacturers recommended procedures.  It is critical to avoid drying electrodes at temperatures above those recommended.  Also, longer hold times at lower temperatures is not equivalent as holding the right temperature for the specified time.  For additional information on storing and re-drying low-hydrogen electrodes read Storing and Re-drying Low Hydrogen Electrodes.

 

Non-Low Hydrogen Electrodes

If exposed to humid air for long periods of time the welding characteristics may be affected.  If moisture appears to be causing problems it is recommended to store open containers in cabinets heated to 100F – 120F.

 

METAL-CORED & FLUX-CORED WIRES

Most manufacturers supply these electrodes in packages that provide proper protection when stored indoors with a relative humidity not higher than 70%.  It is important to store in areas that minimize temperature variations to avoid condensation on the consumables.

 

Storage of Unopened Packages

Store in its original, unopened packaging until it’s time to use.  Protect from condensation and the elements (rain and snow).  For applications in which the weld metal hydrogen must be kept under a specific amount (usually 8mL/100g H2 or lower) only use product supplied in hermetically sealed packaging.

 

Storage of Open Packages

For FCAW and MCAW wires that have been opened follow the recommendations below:

  • Use within a week of opening original packaging
  • Do NOT expose open wires to damp conditions or extreme temperature changes
  • When not in use place wire back in its original packaging (bag and box) and seal as best as possible
  • Discard any wire that has been exposed to moisture and shows signs of rust.

 

Flux-cored wire should not be left out in the open when not in used as it is prone to moisture pick up.

 

SOLID WIRES & GTAW CUT LENGTH

These electrodes are not as susceptible to moisture pick up, but should still be stored in similar fashion as the ones above.  Store in unopened container until it is time to use.  Store in areas protected from rain and snow, avoid severe fluctuations in temperature and protect from condensation.  Discard if wire shows rust on its surface.

References:  AWS D1.1/D1.1M: 2015 Structural Welding Code – Steel

The Procedure Handbook of Arc Welding, 14th Edition

 

Please note: I reserve the right to delete comments that are offensive or off-topic.

Leave a Reply to frankie vaccarella Cancel reply

Your email address will not be published. Required fields are marked *

4 thoughts on “Proper Storage of Welding Consumables

  1. 1. ACCORDING TO AWS D1.1 DOES UNOPENED BOXES OF FLUX CORE WIRE (ESAB DS11 70
    ULTRA 045X33 FLUX CORE WIRE HAVE TO BE KEPT IN AN OVEN??

    2. IF SO, AT WHAT TEMP SHOULD WE STORE THE UNOPENED BOXES OF FLUX CORE
    WIRE??

    3. HOW MANY HOURS CAN WE HAVE IT EXPOSED BEFORE HAVING TO PUT IT BACK IN AN
    OVEN.
    THANKS VERY MUCH

    FRANKIE