Weld inspection should not just take place after welding. Inspection before and during welding is critical.  But what can you inspect if welding has not been performed? Take a look at the checklists below for pre, during and post weld inspection.   Most of these items fall under the responsibility of the welding inspector, but any party involved should participate. The welder has the added advantage of being able to see the molten weld puddle while welding.  Experienced welders will be able to see if the required weld penetration is not achieved, if internal porosity is present, and identify other problems that cannot be detected without destructive testing or non-destructive testing such as radiography and ultrasound.

 

Welders must learn to recognize weld puddle behavior that can indicate potential weld discontinuities or defects.

Welders must learn to recognize weld puddle behavior that can indicate potential weld discontinuities or defects.

Checklist – Before Welding

  • Review drawings and specifications to determine if any special considerations, such as preheat is necessary.
  • Ensure purchased material (base material and consumables) are those which have been specified.
  • Check material test reports and chemical compositions against requirements.
  • Check condition and storage of welding consumables. Low-hydrogen electrodes need special storage to prevent moisture pick up.
  • Check that material fit-up is adequate
  • Check the cleanliness of the joint. Excessive levels of rust, oil, dirt, paint and other contaminants are detrimental to weld quality.
  • Check that proper welding procedures specification and welder qualifications are in place and up to date.
  • If preheat is necessary, ensure it is done and measured correctly.

Checklist – During Welding

  • Check that all parameters stated in the Welding Procedure Specification are being followed. These parameters include items such as wire feed speed, voltage, electrical stickout, welding technique, welding progression, travel and push angles, shielding gas, adequate preheat and interpass temperature (if required), etc.
  • Check individual weld passes. If there is a multi-pass weld make sure each pass is adequate before placing the next weld.  Problems can arise when welding over passes that have excessive convexity, trapped slag at the toes and other inconsistencies.
  • If necessary, check that proper interpass temperature is being maintained. Interpass temperature is usually shown as a minimum, but some cases will also have a maximum interpass temperature.
  • Check for visual cues that can  indicate problems. This is the responsibility of the welder.   Surface contaminants, low-melting elements and other things can cause a variety of problems.  A welder can see if he is not getting adequate penetration, something that can’t be seen after welding unless ultrasonic, radiographic or other NDE tests are performed.

Checklist – After Welding

  • Check weld appearance to ensure no inconsistencies or discontinuities are present.
  • Check for adequate weld size.
  • Check for adequate weld length, especially when intermittent welds are used.
  • Select parts to be tested according to specifications.
  • Check that postweld heat treatment is done properly, if necessary.

A welding inspector cannot reasonably expect to be able to monitor all of this for every single station and weld performed. Therefore, it is critical that welder and other personnel are trained in all aspects of visual inspection.  Identifying problems before welding can save a lot of time and money, do not limit your inspection until after welding.

Do you have any other items that can be added to any of these checklist?

Source: Certification Manual for Welding Inspectors: Fourth Edition (American Welding Society)


Are you tasked with developing, qualifying and approving welding procedures?  Are you in need for procedures that adhere to AWS D1.1 Structural Welding Code – Steel?  If so, the use of prequalified Welding Procedure Specifications will help you save time and money.  It will also help with quality and consistency.  Qualification testing for a single welding procedure can cost over $1,000 depending on the necessary tests.  Prequalified WPSs are exempt from testing and ready to use.

Please note: I reserve the right to delete comments that are offensive or off-topic.

Leave a Reply to Best Cswip 3.1 Training In Hyderabad Cancel reply

Your email address will not be published. Required fields are marked *

7 thoughts on “Inspection Before, During and After Welding is Critical

  1. Dear all, I’d like to get the proper device or instrument the detect welding quality , cracks and shape of it with all details any failure modes will happen, plz price list and technical data, Mohamed
    0120042568

    • It depends on the joint, material, etc. It may require a combination of radiographic, ultrasonic and other NDT methods. You can call the manufacturer of any of this type of equipment and they should be able to help you identify the required equipment as well as provide you with a quote.

  2. Visual inspection of structural steel welding is often misconstrued as part of non-destructive testing (NDT). NDT testing of structural steel in most circumstances is done at the end of the fabrication or erection processes. On the other hand, proper visual weld inspection is not just conducted after the welds are complete. A Certified Weld Inspector (CWI) must begin introducing quality control and assurance measures before a weld takes place, and continue throughout the welding process rather than starting the inspection process upon completion of the project.