How to Weld Austenitic Stainless Steels: The Basics

This introductory post highlights the unique characteristics and importance of austenitic stainless steels, specifically grades 304, 304L, 316, and 316L. It details how alloying elements like chromium and nickel contribute to their excellent corrosion resistance, ductility, and toughness. The article emphasizes the critical role of proper welding procedures in maintaining these properties, especially in preventing issues like carbide precipitation and distortion. It also previews an upcoming collection of prequalified welding procedures for these common stainless steel grades.